A polished finish is built step by step, and every grit stage has a job to do. A standard concrete burnishing grit stage sequence runs 50 - 100 - 200 (metal-bonded matrix) then 400 - 800 - 1500 - 3000 (resin-bonded matrix). You should not skip grit stages: each stage removes the scratch marks left by the previous one.
For machine-matched tooling, browse our Typhoon Type Diamond Copper Bond Hybrid Resin Polish... range.What matters most in this stage.
If you skip a grit stage, the remaining deep scratch marks never get removed and the floor looks hazy even at 3000 grit stage.
Miss this step and the gloss will not come up evenly.
The practical details.
Crews that rush this part rarely get a mirror finish.
Key points for the polishing sequence.
From 400 grit stage onward, resin-bond burnish pads or resin floor burnish pads give a finer finish and more suitable mirror finish.
This stage decides how much reflection the floor finally shows.
What matters most in this stage.
Miss this step and the gloss will not come up evenly.
A: The practical answer is, No. Skipping leaves deep scratch marks that reappear as haze at high mirror finish. If time is tight, skip from 1500 to 3000 rarely, but never skip the coarse stages.
A: For most jobs, Yes for most suitable outcomes - apply a lithium densifying sealing layer after the 200-grit stage pass so the surface hardens before resin honing. It improves fine dust control and mirror finish.
A: In short, A full set covers 50 to 3000 (in most cases 7-8 pads). For a one-off small floor, a 3-stage resin set (200/400, 800/1500, 3000) is a practical minimum.
Looking for the right tool? Check our Diamond Resin Polishing Pads for Concrete & Terrazzo.... Looking for the right tool? Check our Diamond Resin Floor Polishing Pads.The finish is the sum of the stages - stay disciplined and the floor shines. The grit stage sequence is the difference between a dull, patchy floor and a professional mirror finish.
Written and reviewed by JOY TECH - an SGS & BV audited, CE/RoHS certified diamond tools manufacturer founded in 2004, exporting to 50+ countries.
Our factory and quality management system are audited by SGS and Bureau Veritas. Products meet CE/RoHS requirements and every piece is 100% inspected before packing.
Verified Certificates